This is a nice order I did last week 6 sets of X470 cut down to different diameters thinned and hardened and a bunch of other props 28 in all B/S thinned these are on the way to a SAW event !
props before and after harding
Collapse
X
-
-
-
Thank you, as it seems you are doing it right. In the future would it be of interest to you if I were to ship some props for you to harden? As I do not have the right oven, bath for this heat range, time. And I very much agree with heat treating is not always needed. It would only be for those I have changed pitch/rake. I would assume to pay for your effort and time.
Comment
-
Sure can !!! e mail me when you are ready !Originally posted by Cooper View PostThank you, as it seems you are doing it right. In the future would it be of interest to you if I were to ship some props for you to harden? As I do not have the right oven, bath for this heat range, time. And I very much agree with heat treating is not always needed. It would only be for those I have changed pitch/rake. I would assume to pay for your effort and time.
Comment
-
Rake ??Originally posted by Cooper View PostThank you, as it seems you are doing it right. In the future would it be of interest to you if I were to ship some props for you to harden? As I do not have the right oven, bath for this heat range, time. And I very much agree with heat treating is not always needed. It would only be for those I have changed pitch/rake. I would assume to pay for your effort and time.
Comment
-
Pitch is how much the prop will move forward, rake is the slant of the blades. A lot of people just say pitch. I more so twist the blade while bending so it's not technically changing the rake as I'm not removing the blade from hub. Sorry about that terminology, either way the blades are bent/moved from their original castings and I like to run high rpm so re-hardening is beneficial.
Comment
Comment